Mine's a flattened nozzle from 1/4 copper tube, trying to achieve a fan spray close to the point of contact. Flood to wash away the crud. I prefer grinding dry but it puts gritty dust into the air.
12-18-2015, 07:47 PM
Never thought of using copper tube. I was going to make one out of some hex brass I have. That's much easier! The pump won't be here till next week anyway and I can save that brass for better things.
Thanks!!
Thanks!!
12-18-2015, 10:50 PM
I prefer to grind dry as well. It's a lot less hassle to hook up a dust collector than deal with the mess that coolant makes.
Tom
Tom
12-19-2015, 10:50 AM
One thing that occurred to me. The last time I ground something it turned a little brown, my thought was "wrong wheel" but perhaps I should have turned on the coolant. Effectively turning the one wheel into two.
12-19-2015, 06:43 PM
I've worked in a number of grinding shops almost none of them used coolant on the surface grinders. If you are generating enough heat to turn the part brown, there are a number of things that can be done to reduce it. Moving to a softer, more friable wheel will help, as will decreasing the depth of cut and increasing the feed rate. A lot of side movement of the wheel helps as well, as in 3/4" overlap with a 1" wheel (light cuts of course). Quickly covering the entire surface of the part means more heat in the chips and less in the part.
Tom